Tech sheet says that sealed container should not exceed 7 days....I have a container that has been out for nine days, what do you think????? Has anyone any similar experience or pointers ??

reply »

steve

#34256

ALPHA WS-709 | 16 May, 2005

I see what you mean. Personally I would try a bit of the paste and see what you think prior to production run. If I were you I would get another brand in there. something that offers a "slightly" longer life? I have used "out of date" solder paste many times and experienced few if any problems. I guess it's like the experation date on food. Recommended but not exact.

reply »

#34257

ALPHA WS-709 | 16 May, 2005

We agree with an earlier poster. Try it and carefully observe the results.

We agree with earlier comments. Consider a paste with a more current design. WS709, while SOA in it's day and still a very good paste, is dated.

reply »

#34261

ALPHA WS-709 | 16 May, 2005

Dave,

When you say "we", who do you mean ? The company you work for ?

Just curious. Thnx, Sr.

reply »

#34290

ALPHA WS-709 | 17 May, 2005

Never mind then.

Must be the Borg collective you are speaking of.

reply »

KEN

#34306

ALPHA WS-709 | 17 May, 2005

...circa 1996.