Reflow Pallet hardware

#34455

Reflow Pallet hardware | 24 May, 2005

Hi All,

I am looking for a supplier for the hardware used on reflow SMT carrier pallets. I know that there are many vendors who can make the pallets themselves, but where do they get the locator pins or spring clips. I'm not sure if each vendor just has them custom made or not. We have a tool shop in house that could make them but I figured i'd check to see if there was a vendor.

I am specifically looking for the type of spring clips that hold a PCB in a carrier below or even with the surface to allow screen printing.

thanks

reply »


RDR

#34457

Reflow Pallet hardware | 24 May, 2005

Try Pentagon-ems.com (might be right address?) They make their own hardware and i have purched various odds and ends from them before. Ask for Chad Haima.

reply »

#34465

Reflow Pallet hardware | 25 May, 2005

We also want to use pallet method. How you work it out. We do have small PCB ( 30mm x 50 mm ) which have 0402 component & also micro BGA. Is it possible to make pallot for these component. thanks Ajay

reply »


RDR

#34467

Reflow Pallet hardware | 25 May, 2005

Send your gerber data to the above mentioned or any other pallet Mfgr. If the assembly is designed with pallets in mind I am sure that one can be designed for your application.

reply »

#34468

Reflow Pallet hardware | 25 May, 2005

For pallet hardware try: * Summit Precision 5825 S 25th St, Phoenix AZ 85040 Dennis Miller 602-268-3550 http://www.summitprecision.com sales@summitprecision.com

* Southco http://www.southco.com

reply »

PW

#34469

Reflow Pallet hardware | 25 May, 2005

In a time crunch, kapton tape works great. If you are using durostone or some material like that for carriers, make sure it is clean right after you machine it and the kapton will stick very well. We are low volume so we pretty much always use tape to simplify fixture design. Off the subject some but; non-photo reflective durostone is cheaper than reflective and you can simply spray paint a stripe of high temp. white paint where your sensors need to see your carrier. Hope this help a bit!