I have a large (25" width x 14" length) PCB that's getting ready for production. Our current paste printing equipment will not handle this size board. Does anyone out there know of a semi-auto paste printing or paste dispensing machine that can handle this size board?

How are you folks printing large boards?

Thanks.

reply »

#35867

Large PCB Paste Printing | 3 August, 2005

Hi

Here is one that can handle the size board that you are looking to print.

http://www.reprintservices.co.uk/R29_Series_Screen_Printer.html

Hope that this is of help.

Regards

Ian

reply »


Rob

#35872

Large PCB Paste Printing | 3 August, 2005

There's always a used MPM UP3000, they're cheap.... ....but there is a very good reason for this.

reply »

#35880

Large PCB Paste Printing | 3 August, 2005

Ekra makes a printer than can do 25".

reply »


Rob

#35882

Large PCB Paste Printing | 3 August, 2005

Hey Dave,

Congratulations on hitting 4000!

Treat yourself to a tiepin.

Cheers,

Rob.

reply »

#35886

Large PCB Paste Printing | 3 August, 2005

Holy crap !

4000. Now that's old !

reply »

OverTheHill

#35894

Large PCB Paste Printing | 3 August, 2005

Many thanks for the info folks.

reply »

#35961

Large PCB Paste Printing | 8 August, 2005

MPM SPM semi-automatic printer can handle up to 26.5" x 21" max. PCB

MPM UF3000 automatic, up to 27" x 20"

MPM AccuFlex automatic, up to 23" x 20"

For more info:

http://www.speedlinetech.com/mpm/index.aspx