Flex testing of PCBA

Views: 1522

Woodsmt

#36124

Flex testing of PCBA | 15 August, 2005

Does any one know of a Lab which performs mechnical flex testing of boards? I have a problem with ceramic devices cracking, and need to determine how much flex is ocurring to help in stiffiner designs. It would be helpful if the Lab is in the New England area, but not required.

This message was posted via the Electronics Forum @

reply »

#36315

Flex testing of PCBA | 25 August, 2005

Voidless Reflow Soldering

TWEEZER-VAC ELITE Vacuum SMD Tweezer Kit