We are experiencing cracking of 1206 .1uf/50V capacitors on ...
- Aug 30, 2005
by
esoderberg
Check them before the oven for cracks. (after placement) Don...
- Aug 30, 2005
by
Stephen
Describe the location and orientation of the cracks.
...
- Aug 30, 2005
by
davef
...
- Aug 31, 2005
by
I just had a "how could I have forgotten" moment.
By any ch...
- Aug 31, 2005
by
Stephen
or damaged on breakout - especially if the V score is non co...
- Aug 31, 2005
by
Rob
We had a problem with cracked caps a few months ago,they wer...
- Sep 01, 2005
by
just at 0.200 from both the short and the long edge
...
- Sep 06, 2005
by
esoderberg
Have experienced this on a few different cap. parts. Agree ...
- Sep 07, 2005
by
or the biggest issue from my days with the worlds largest Ch...
- Sep 07, 2005
by
Rob
This pattern indicates flex cracking due to excessive bendin...
- Sep 09, 2005
by
davef