solder paste mixing | 26 September, 2005

I am looking for input on a solder paste mixer for 500g jars. Does anyone have a good recommendation? Thanks

reply »

#36901

solder paste mixing | 30 September, 2005

Good day,

Check this out: http://www.mvent.com.ph/malcom/sps1.htm. SPS-1 is rather good.

BR, Pavel

reply »

#36907

solder paste mixing | 30 September, 2005

Solder Paste Mixer * Malcom [malcomtech.com] SPS * Japan UNIX [japanunix.co.jp] Uni-Cyclone UM-103 * Genitec [genitec.com] GAM60 * Synergy Engineering [synergymark.com] Unity 500J