Hi,
I see that the wave angle of the wave solder machine ...
- Nov 05, 2005
by
Milroy
Typical is 4 to 6 degrees inclination.
...
- Nov 05, 2005
by
Hi Ken
What exactly the best reffered angle for Sn/Pb & P...
- Nov 06, 2005
by
Milroy
About the anlge typically is 5-7 depending on the machine. ...
- Nov 07, 2005
by
LUPO
6 deg is std angle. Some machines have option to adjust angl...
- Nov 07, 2005
by
PeteC
Milroy,
Another thing to look at is your wave profile. Che...
- Nov 10, 2005
by
Hi,
I`m thinking what would be the best way to avoid icic...
- Nov 16, 2005
by
Milroy