Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Wave Soldering / Masking PEM Hardware

Views: 1651

B. Tamland

#37902

Wave Soldering / Masking PEM Hardware | 16 November, 2005

Has anybody had to wave solder components after PEM hardware has been installed to the wave side of the board? Design constraints on the product force us to do this, and we need to determine a method to mask the PEM's. Anybody try hi-temp boots / CAP-Lugs? Thanks

reply »


URL

#37935

Wave Soldering / Masking PEM Hardware | 17 November, 2005

yeah, i tried um once and they worked great. gwad dam management wouldnt buy em though.

reply »

Burgandy

#37942

Wave Soldering / Masking PEM Hardware | 17 November, 2005

This process damn near ruined mah career.

reply »

Kornholio

#37943

Wave Soldering / Masking PEM Hardware | 17 November, 2005

I purchased them too but it was a conspiracy that they didn't work because an operator told management and he took all the credit.

reply »


RDR

#37950

Wave Soldering / Masking PEM Hardware | 17 November, 2005

If you only need to keep the threads clear you can use nylon screws and then remove them after they get cool.