Plasma nitride wave solder pot lining for lead-free use | 5 December, 2005

I searched the archives, found one thread with one response (my own, which went unnoticed since this forum doesn't bump threads when they get responses), so I'm hoping a resurrection of sorts will generate some input.

Anyone using one of these systems or heard any good/bad/ugly stories about reliability, longevity, etc.?

reply »

Adnahn

#38411

Plasma nitride wave solder pot lining for lead-free use | 13 December, 2005

Hi Steve,

What I came up with for our Soltec Sigma 6621 is to make a stainless steel wave solder bath insert.The insert with all its components eg. impeller, Chipwave assy, pump shafts, main wave assy etc. I will send for plasma nitride coating.Afer installation I will do a six month periodic inspection for the 1st 2 years to monitor the durability of the coating.

Regards Adnahn