Does anyone have any insight as to the cause of cracked chip...
- Feb 28, 2006
by
jagman
Depaneling with the parts in question near a V-score?
...
- Feb 28, 2006
by
Steve Thomas
Too fast heating/cooling rate in reflow (look at mfg's spec....
- Feb 28, 2006
by
Steve,
I believe you hit it right on the head! Thanks!
...
- Feb 28, 2006
by
jagman
PWH,
Thanks for all your input. All these areas are of c...
- Feb 28, 2006
by
jagman
Round cracks that look like it's from a placement are genera...
- Mar 01, 2006
by
jagman,
take a hard look at a capacitor under the high ma...
- Mar 02, 2006
by