Dross removal

Views: 3834

#40306

Dross removal | 8 March, 2006

Several weeks ago, there were some postings about a new product for reducing dross in the wave solder pot. It was, I think, a liquid. Both for Tin/Lead and lead free solder. Anyone remember who this vendor is?

reply »

Cal Kolokoy

#40307

Dross removal | 8 March, 2006

The vendor is PK Metals. Their product is called molten solder surfactant.

reply »

#41286

Dross removal | 2 May, 2006

Hi Anyone has used Kera-clean Dross Ex to clean the dip soldering nozzle before?

This product is from Kera-Technik@gmx.de, GmbH, Germany, and has been quite effective in removing the dross residue on the nozzle.

Tell me is there a similiar product in the US?

rdg george

reply »

#41484

Dross removal | 11 May, 2006

The MS2 Molten SOlder Surfactant web site is http://www.pkaymetal.com The product is not commercially available.

reply »

hector.iduma@ge.com

#44729

Dross removal | 26 October, 2006

PK METALS in California PRODUCT MS2

Ing. Octavio Raygoza PKay Metal sales manager tel. 011 52 (619) 666-5795

reply »

#44744

Dross removal | 27 October, 2006

I use adipic acid to clean our Ersa selective solder machine nozzles. Makes a huge difference and is quick and easy.