Any recommendations on selective l/f soldering equipment for low volume high product mix applications.

reply »

#43880

Selective Soldering | 12 September, 2006

We're using a Pillarhouse for all of our Pb free. JADE I believe is the model. Good little machine, pretty easy to program and maintain.

reply »

C Curk

#43889

Selective Soldering | 12 September, 2006

You should look into the ACE Unit. Best unit on the market. Sells complete for $55,000. HAndles a 18 x 24 board, 1MM keep away area. Made in teh U.S. too. Email me at clcurk@att.net I can email you a link to the site.

reply »

#43891

Selective Soldering | 12 September, 2006

#44036

Selective Soldering | 19 September, 2006

Hi there, we use inertec els 3.0 and 4.0 machines regards

reply »

egrice1@wi.rr.com

#44138

Selective Soldering | 25 September, 2006

Check out ERSA's Ecoselect 350. You can have 2 solder pots in the machine. 1 for SN/PB and 1 for Lead Free.

It's a little more than $ than the others, but its a production machine! Not a toy.