lead free vitronic(s) profile | 12 December, 2006

As we have vitronics oven(SMR610A) made in dec,1997,which has 5 heating zones and 2 cooling zones. For Lead free soldering what should be our baseline for low/medium boards.we have gathered profiles from various paste manufacturers,however we don't know any data. what temperature should be kept at heating zones and cooling zones?

reply »

#46173

lead free vitronic(s) profile | 14 December, 2006

Use the thermal recipe suggested by YOUR paste supplier, as the starting point.