change process Epoxy before solder past

Views: 1968

josaf

#46349

change process Epoxy before solder past | 22 December, 2006

Can I change process from solder paste [ Top sode ]-- > Epoxy [ bottom side ] to

Epoxy [ bottom ] ---> solder paste [ top side ]

reply »

#46352

change process Epoxy before solder past | 22 December, 2006

Good afternoon,

Yes, you can. But what for?

BR, Pavel

reply »

#46358

change process Epoxy before solder past | 22 December, 2006

Epoxy [ bottom ] ---> solder paste [ top side ]

Actually it's kinda the norm in most places. Subjects your active components to one less heat cycle.

reply »

Jav Thug

#46360

change process Epoxy before solder past | 22 December, 2006

Niiiice process

reply »

#46368

change process Epoxy before solder past | 23 December, 2006

Of Course you can. We have a customer specific board that has a stupid connector underneith, and we must manually glue this one onto it's postition before reflow on the secondary side first... And as you know, the customers is alwayw left... The funny thing is: Only chips on the primary side...But they are paying us for this stupid behaviour...

Ps. Don't tell anybody, but I have almost secretly been able to change the process in the oppossite way, our operators doesn't care but they think this is a bit of fun...We still doing the glueing process though. We all need some laughter once in a while. Ds.