best foam flux for pb-free wave soldering with alloy Sn100 | 4 April, 2007

Hi, colleagues! We only start using pb-free tehnology Our wave have foam fluxer What kind of flux would be best if we will use Sn100 solderbar What is your experience Best regards Peter

reply »

#48866

best foam flux for pb-free wave soldering with alloy Sn100 | 4 April, 2007

Indium Corp. has some, 3549-HF and 3590-T, both are OK for foaming. Most of the better performing newer fluxes require spray application for best performance. Alpha, Kester and others have wave fluxes too.

http://www.indium.com/products/circuitboardassembly/wavesolder.php