Acrylic conformal coat cure test method

#5414

Acrylic conformal coat cure test method | 28 February, 2001

Checked the archives with no luck. Anyone have a reliable test method of verifying acrylic conformal coat cure. Using Humiseal 1B31 mixed with approximately 30% solvent, spraying with a Nordson. Thanks in advance.

reply »

#5415

Acrylic conformal coat cure test method | 28 February, 2001

Checked the archives with no luck. Anyone have a reliable test method of verifying acrylic conformal coat cure. Using Humiseal 1B31 mixed with approximately 30% solvent, spraying with a Nordson. Thanks in advance.