Cleaning Wave solder fingers and chain | 26 August, 2008

The chain and fingers for our Wave solder is getting a large amount of residue from the flux (high dissolved solids) we are using. Any recommendations for products that can clean polymerized flux.

reply »

#56181

Cleaning Wave solder fingers and chain | 26 August, 2008

What brand of flux and wave solder machine are you using?

George

reply »

#56191

Cleaning Wave solder fingers and chain | 27 August, 2008

We are using Multicore (MFR 301) from Henkel.

reply »

#56205

Cleaning Wave solder fingers and chain | 27 August, 2008

We roll ours up, fingers and all, and soak them for about an hour in a solution of water and DOMINATE (heavy duty degreaser) you can order from Grainger. They come out looking brand new every time!

reply »

#56207

Cleaning Wave solder fingers and chain | 27 August, 2008

We use a power washer, blow dry, then lightly oil the links with mineral oil. Works great