Dr Lee: What are your recommendations and sources of excellent publications and books on solder paste printing?

reply »

Dr. Ning-Cheng Lee

#6287

Re: Solder Paste Printing Text | 23 August, 2000

Regarding solder paste printing, many books available on the market all have some sections addressing this topic. Unfortunately, as of today, solder paste printing has not been the main theme of any book yet. I consider the better sources of information on printing would be some short courses offered at trade shows such as SMTA International, IMAPS, or Nepcon West.