Cleaning Misprinted PCB's | 20 July, 2000

What is the preferred method of cleaning misprinted double sided No-Clean boards which are assembled on side 1 ? What type of equipment is being used ? What solvents / detergents work well for a variety of solder pastes / glues ?

reply »

Bob Willis

#6339

Re: Cleaning Misprinted PCB's | 21 July, 2000

There is no easy answer to this as no one wants to do it.

There are lots of systems out there but cleaning dried paste is an issue and getting paste out of holes. You should speak to the paste and adhesive supplier to check on soluability of materials.