ISOLA 410 laminate | 27 May, 2011

Hi all,

Looks like this laminate is becoming extinct... What have you switched to if you were a user?

AJ...

reply »

#64394

ISOLA 410 laminate | 1 June, 2011

Hi Aj,

for the most part we have gotten away from calling out specific material and instead calling out IPC4101 back slashes to needed requirements.

But if you are just looking for what most domestic shops have switch to you would be looking at 370HR Isola. on the Offshore side it would be Iteq IT180 or Grace GA-170.

Regards, Mike