Does anyone know of a company who can repair and straighten the leads on QFP's? We have quite a few parts that were received with bent leads.

reply »

Steve Gregory

#7119

Bent leads on QFP's | 29 June, 2001

Hi Ed!

A company that I've used in the past and is very good is Six Sigma in San Jose, California. Their web page is at:

http://www.sixsigmaservices.com/

-Steve Gregory-

reply »

Steve Gregory

#7120

Bent leads on QFP's | 29 June, 2001

Hi Ed!

A company that I've used in the past and is very good is Six Sigma in San Jose, California. Their web page is at:

http://www.sixsigmaservices.com/

-Steve Gregory-

reply »

#7132

Bent leads on QFP's | 30 June, 2001

Sohowcum, yer not just sending the bent-up leaded QFP back to the sorry behinds that sent them to you and telling �em they aint no good!!! Gimme goodins!!! [Er, words to that effect.]

For QFP lead reconditioning equipment suppliers, try: * Knight Tool 978-373-1807 Bill Einhorn * Fancort 800-554-9773 Chuck Bowman * Dana Design 707.778.3113 fax 3190 * Precision Technologies Santa Clara, CA * Topline 714 898 3830 [Are they still in business? There has been some tribal warfare, but ] * SESA 1700 Wyatt Dr Suite 11 Santa Clara CA 95054 408-988-5816 fax 5817 pgd@sesa.com

For QFP lead reconditioning services try: * Corfin 603-893-9900 * Six Sigma (408)526-1350 x 1