Hello
I have the problem with selective soldering on the ro...
- Jun 20, 2017
by
ranap121212
I would start with checking the flux amount and trace and th...
- Jun 21, 2017
by
Evtimov
but we do not have laminate preheating on robots. There is n...
- Jun 21, 2017
by
ranap121212
Try baking the boards; you may have a moisture problem.
...
- Jun 21, 2017
by
mac5
Are you using nitrogen in your soldering process?
...
- Jun 22, 2017
by
CAPSE
There are several different technologies in the industry tod...
- Jun 22, 2017
by
SolderingPRO
Thanks from your answer. A few days ago the supplier told me...
- Jun 24, 2017
by
ranap121212
@Capse, No but the machine has such a construction, I can no...
- Jun 24, 2017
by
ranap121212
If N2 is not an option, the cut wire feeder or drilled wire ...
- Jun 26, 2017
by
CAPSE