Alloy melting Points | 5 November, 1999

What is the liquidous temp for: 95Sn/5Ag and 96.5Sn/3.5Ag

thanks in advance

reply »

#8660

Re: Alloy melting Points | 5 November, 1999

Brian,

96.5Sn/3.5Ag is eutectic at 221 C

95Sn/5Ag has a melting range of 221 - 240 C

Hope that helps you out...

reply »

Jeff Sanchez

#8661

Re: Alloy melting Points | 5 November, 1999

Hi Brian, Here is the web address for Indium. If you go to the "technical papers" and then to "specialty solders and alloys" they have a really great chart that has all the alloy specs. Well worth printing. ........Jeff Sanchez

reply »

Jeff Sanchez

#8662

Re: Alloy melting Points, This one has it | 5 November, 1999

Hi Brian, Here is the web address for Indium. If you go to the "technical papers" and then to "specialty solders and alloys" they have a really great chart that has all the alloy specs. Well worth printing. ........Jeff Sanchez

reply »

Jeff Sanchez

#8663

Re: Alloy melting Points, This one has it | 5 November, 1999

Man oh man, ok so cut to the chase.lol www.indium.com

reply »

Comprehensive Analytical Services and Support

Comprehensive Analytical Services and Support