VOC free Flux in Inert Wave Solder Machine

Raeto Zryd

#10594

VOC free Flux in Inert Wave Solder Machine | 15 July, 1999

We intend to use VOC free fluxe in our nytro machine. Does anybody know if there can be problems with water ie. solvent residues in the tunnel. Perhaps there are some white papers available on that issue.

reply »

Vic Lau

#10595

Re: VOC free Flux in Inert Wave Solder Machine | 16 July, 1999

| We intend to use VOC free fluxe in our nytro machine. Does anybody know if there can be problems with water ie. solvent residues in the tunnel. Perhaps there are some white papers available on that issue. | | | | | Dear Raeto,

In my experience, I find no big problem on using VOC-free flux in an inert atmosphere wave soldering machine. However, if wanted, you can go to the kester website, www.kester.com or alpha metals website, www.alphametals.com. There are some technical papers about VOC-free fluxes.

Vic Lau

reply »