Castin | 29 June, 1999

Does anybody have experience with this supposed drop-in replacement for lead solder. I checked out the tech sheets on this product and it seems to check out. I could not find any information about Lucent's research on it, although I was not exactly sure where to find it. I will attach the link so that any ptential problems may be addressed. Is this stuff as good as it sounds? Are there other near eutectic drop-ins for lead solder?