Re: Reliability data on pressfit rework/repair. | 30 January, 1999

Does anyone have any reliability data /concern on pressfit rework/repair - is there any qualified /characterized equipment /tools present in the industry? What kind of effect does it have on barrel plating quality (1.5mil avg.) after 1 time rework or pressfit connector pullout process. Thanks in advance for help.

reply »

Justin Medernach

#12754

Re: Reliability data on pressfit rework/repair. | 2 February, 1999

| Does anyone have any reliability data /concern on pressfit rework/repair - is there any qualified /characterized equipment /tools present in the industry? | What kind of effect does it have on barrel plating quality (1.5mil avg.) after 1 time rework or pressfit connector pullout process. Thanks in advance for help. | The data you ask for is fairly difficult to ascertain. The pin composition, barrel composition, barrel diameter, pin diameter, and pin geometry will all have a differing effect on the barrel integrity after pressing. In house, we have a rule. Replace it three times and the fab is scrap. this seems to work fairly well as we haven't had any reported failures attributed to the press fit operation.

Regards, Justin Medernach