SRS Machine Issue..What about the dross recycling | 28 December, 1998

We are looking into a SRS machine, and one question keeps coming up, "If we pull out all the solder, will the recycling company refuse to purchase the remaining dross?"

Anyone who out there that uses a SRS machine(Solder Recovery System) I would appreciate any information on this. Did they reduce the amount that they paid for the dross? Did they refuse to buy it? Did they reduce any services to your organization?

A big thank you in advance!!!!!

reply »

Darryl Schlosser

#13196

Re: SRS Machine Issue..What about the dross recycling | 29 December, 1998

| We are looking into a SRS machine, and one question keeps coming up, "If we pull out all the solder, will the recycling company refuse to purchase the remaining dross?" | | Anyone who out there that uses a SRS machine(Solder Recovery System) I would appreciate any information on this. Did they reduce the amount that they paid for the dross? Did they refuse to buy it? Did they reduce any services to your organization? | | A big thank you in advance!!!!! | I have been using a SRS machine for about 1 year. Dross prices remained the same. Dross quantity was cut in half. You cannot dump dross out of your solder pot that is laden with good solder. The trick to using the machine is to only scoop the black powder into the machine. e-mail for more info.