Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Solder Stack Film Capacitors

dpoling

#2619

Solder Stack Film Capacitors | 27 October, 2000

We are currently having problems with tombstoning and minor lifting on small SMT stasck film capacitors. Does anyone have any ideas?

reply »

Aaron

#2620

Re: Solder Stack Film Capacitors | 28 October, 2000

1. Check printing accuracy. 2. Check placement accuracy. 3. Your components should be kept in a good environment to prevent oxidation of terminations. 4. Pads pattern should be designed according to standards.

If 1.2. are okay, you should suspect 3.:oxidation. Conveyor speed of oven may not be a big fact, for the part is very small.

Good luck.

reply »

SMT fluid dispensing

Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes