Solder Paste process with PHT components?

Sandro R. dos Prazeres

#14973

Solder Paste process with PHT components? | 17 July, 1998

Is there anybody with knowledge in the process with PHT components (Components with terminals) - Cause with make board with top and bottom side, with SMD and Auto Insertion Technology. So we want to do a Entire Cell with both technology, and without Wave Solder...So, if somebody could help me.

reply »

Sergio Corcuera

#14977

Re: Solder Paste process with PHT components? | 17 July, 1998

| Is there anybody with knowledge in the process with PHT components (Components with terminals) - Cause with make board with top and bottom side, with SMD and Auto Insertion Technology. So we want to do a Entire Cell with both technology, and without Wave Solder...So, if somebody could help me.

reply »

Sergio Corcuera

#14978

Re: Solder Paste process with PHT components? | 17 July, 1998

| | Is there anybody with knowledge in the process with PHT components (Components with terminals) - Cause with make board with top and bottom side, with SMD and Auto Insertion Technology. So we want to do a Entire Cell with both technology, and without Wave Solder...So, if somebody could help me. | | We are running a board using pth components and also SMT on both sides (bottom and Top), whithout solder wave machine on line, we have two reflow process (one for bottom and other for top), what's seems to be the problem for you?, we mount pth components and SMT IC's on top during second reflow. If you need more information e-mail me and maybe i can help

reply »

Russ Miculich

#14976

Re: Solder Paste process with PHT components? | 22 July, 1998

Yes, there is a way to print solder paste into through holes as well as for SMT devices. I suggest you contact Alden Johnson at MPM in Franklin, MA (website info at http://www.mpm.com) about what he has done here. The trick in getting the solder paste in the hole is how the stencil is cut, how thick it is, and use of either a rheological pump or pneumatic paste printer to push the solder into the stencil apertures and into the holes on the board. Printer manufacturers offering this technology are SMTECH, MPM, and DEK. | Is there anybody with knowledge in the process with PHT components (Components with terminals) - Cause with make board with top and bottom side, with SMD and Auto Insertion Technology. So we want to do a Entire Cell with both technology, and without Wave Solder...So, if somebody could help me.

reply »

Dave F

#14975

Re: Solder Paste process with PHT components? | 22 July, 1998

| Is there anybody with knowledge in the process with PHT components (Components with terminals) - Cause with make board with top and bottom side, with SMD and Auto Insertion Technology. So we want to do a Entire Cell with both technology, and without Wave Solder...So, if somebody could help me. Sandro: Check this thread out. Dave F Using solder paste/reflow for leaded thru hole parts . - Upinder Singh 11:33:30 7/01/98 (1)

reply »

Jim McLenaghan

#14974

Re: Solder Paste process with PHT components? | 31 July, 1998