White Adhesive Glue

Mohamed Ragai

#15308

White Adhesive Glue | 22 June, 1998

Dear Sirs, I need somehelp to know some sources for white epoxy UV curing SMT adhesive glue ( not alphametal and heuareus ) ,Please help with companies names and tel/fax numbers !! Thanks all Mohamed Ragai

reply »

Dave F

#15310

Re: White Adhesive Glue | 22 June, 1998

| Dear Sirs, | I need somehelp to know some sources for white epoxy UV curing SMT adhesive glue ( not alphametal and heuareus ) ,Please help with companies names and tel/fax numbers !! | Thanks all | Mohamed Ragai Mohamed: I'm not positive if all of the following sources supply white UV adhesive ... some may be clear. Dave F Dymax 860.482.1010 fax 495.0608 Martine Boutte Master Bond 201.343.8983 Permabond 800.653.6523 Hardman 800.321.3572 Loctite 860.571.5100 fax 5465

reply »

Russ Miculich

#15309

Re: White Adhesive Glue | 25 June, 1998

I would suggest you call Dymax (may be Diemax) - they are the adhesive experts when it comes to UV curing materials. I am very sorry, but somehow they are not in my database. You should be able to find them on the net under and adhesives+UV search. If you need further help shoot me an email at r.miculich@smtech.com. You might also talk to Locktite, Masterbond, and Tracon. Good places to start. end of line | Dear Sirs, | I need somehelp to know some sources for white epoxy UV curing SMT adhesive glue ( not alphametal and heuareus ) ,Please help with companies names and tel/fax numbers !! | Thanks all | Mohamed Ragai