| I am looking for alternate suppliers of Hollis wave solder fingers other than Speedline(Electrovert) The Model and S/N of the wave solder is | Model 207944 | Serial # F11132 | Please let me know if you are a vendor or know of a vendor. Your help would be greatly appreciated. Chris: Here's a source for wave fingers. I don't if they have fingers for your machine. Dave F Garland Service, Garland TX 972.494.1911 fax276.0972

reply »

Ken Chase

#15343

Re: Hollis Future 1 wave solder fingers | 23 June, 1998

Yes, New Era Technology, Inc. is a manufacturer of Titanium fingers for Hollis and Sensbee wave Solder machines, as well as a other products. give them a call @ (603)669-7971 for more info.