I have a need to have a number (approx 20) circuit card assemblies which need to have a silicone conformal coating applied per MIL-I-46058. Are there any facilities which can offer me this service? Thank you, Chris Fontaine (603)885-6839 Sanders, a Lockheed Martin Co. P.O. Box 868, NHQ4-1423 Nashua, NH 03061-0868

reply »

Mike Moninger

#16315

Re: Silicone Conformal Coating | 8 April, 1998

| I have a need to have a number (approx 20) circuit | card assemblies which need to have a silicone conformal | coating applied per MIL-I-46058. Are there any facilities | which can offer me this service? | Thank you, | Chris Fontaine | (603)885-6839 | Sanders, a Lockheed Martin Co. | P.O. Box 868, NHQ4-1423 | Nashua, NH 03061-0868 We offer conformal coating services and would be happy to quote your boards. Mike Moninger Thermospray Company, Inc. 1-800-952-5838

reply »

Mike Moninger

#16314

Re: Silicone Conformal Coating | 8 April, 1998

| I have a need to have a number (approx 20) circuit | card assemblies which need to have a silicone conformal | coating applied per MIL-I-46058. Are there any facilities | which can offer me this service? | Thank you, | Chris Fontaine | (603)885-6839 | Sanders, a Lockheed Martin Co. | P.O. Box 868, NHQ4-1423 | Nashua, NH 03061-0868 We offer conformal coating services and would be happy to quote your boards. Mike Moninger Thermospray Company, Inc. 1-800-952-5838

reply »

Bob Barr

#16313

Re: Silicone Conformal Coating | 14 April, 1998

Chris, You may wish to contact Colin Burnie at SigmaVI in Melbourne, FL at 407-255-3559. They have coated boards for me using acrylic with very good results. I can't remember though if they do silicone. They have no problem with small lot sizes. Bob

| I have a need to have a number (approx 20) circuit | card assemblies which need to have a silicone conformal | coating applied per MIL-I-46058. Are there any facilities | which can offer me this service? | Thank you, | Chris Fontaine | (603)885-6839 | Sanders, a Lockheed Martin Co. | P.O. Box 868, NHQ4-1423 | Nashua, NH 03061-0868

reply »

dual pot selective soldering

ADJUST-A-VAC Vacuum Tweezer for fragile components, wafers, MEMS devices tweezers