I require a Template for an internal Solder Paste Stencil Specification. If any one has ANYTHING, could you please reply. Graham

reply »

Scott McKee

#17014

Re: Solder Paste Stencil specifications | 31 December, 1997

| I require a Template for an internal | Solder Paste Stencil Specification. | If any one has ANYTHING, could you please reply. | Graham My suggestion would be to contact your stencil manufacturers. They've seen it all and know more than most... Ask them for their guidelines and modify to fit your spec format. Good luck, Scott

reply »

Paul R. Graham

#17015

Re: Solder Paste Stencil specifications | 6 January, 1998

| | I require a Template for an internal | | Solder Paste Stencil Specification. | | If any one has ANYTHING, could you please reply. | | Graham | My suggestion would be to contact your stencil manufacturers. | They've seen it all and know more than most... | Ask them for their guidelines and modify to fit your spec format. | Good luck, | Scott Thanks

reply »

Steve Gregory

#17012

Re: Solder Paste Stencil specifications | 23 January, 1998

Paul, I've got a third-level ISO Stencil Specification procedure that I did at a past employer that I'll send you...it also deals with the DEK-265 printer (which is what we used) when I talk about frame sizes and image positioning, but you can edit it to whatever printer you guys use. Steve Gregory Zevatech Inc.

reply »

fxb

#17013

Re: Solder Paste Stencil specifications | 23 February, 1998

| Paul, | I've got a third-level ISO Stencil Specification procedure that I did at a past employer that I'll send you...it also deals with the DEK-265 printer (which is what we used) when I talk about frame sizes and image positioning, but you can edit it to whatever printer you guys use. | Steve Gregory | Zevatech Inc. Would you give me the same material for me ? thank you very much Jerry Wei

reply »

ADJUST-A-VAC Vacuum Tweezer for fragile components, wafers, MEMS devices tweezers

conformal coating pcb - asymtek