Kyzen vs Zestron - Which is better? | 1 August, 2002

We've been running Kyzen XJN+ with our new Westek Trek IV cleaner for months and have had few problems with ionic contamination. Prior to that we've used Kyzen products forever. Recently a Zestron rep did a sales pitch claiming a 50% savings if we switched to Zestron Vigon A200. Does this sound right? Sounds like everyone would be using Vigon if it were that simple. Please comment. Thanks in advance.

reply »

#21031

Kyzen vs Zestron - Which is better? | 1 August, 2002

Don't know about the savings over Kyzen, but from my experience Zestron Vigon A200 at 12% concentration in the wash tank delivered excellent cleaning results- even on some NC fluxed paste. Maybe its a price issue?

reply »

#21033

Kyzen vs Zestron - Which is better? | 2 August, 2002

If I'm not mistaken, XJN is an inorganic highly ionic saponifier. If not completely rinsed off, I would expect that you would get ionic residue.

reply »