Looking for feedback from anyone that is currently screen printing adhesive and having good results. If results are good, what type adhesive and type machine is being used?

reply »

#23384

Screen printing adhesive | 13 February, 2003

We currently screen print all of our adhesive applications and generally have favorable results. The adhesive we use is:

Heraeus , P/N 250 GM Prod/N PD955PR

We print this on three different screen printers, Dek 265 Horizon, Fuji GSP-II and MPM-3000UP We apply the adhesive just as we would paste and like I said generally turn around good results.

Hope this helps, G.Haynes

Vortex@smtnet.com

reply »

#23385

Screen printing adhesive | 13 February, 2003

Heraeus Inc. Circuit Materials Div, 24 union hill rd. West Conshohocken, PA 19428 (610) 825-6050

reply »

#23398

Screen printing adhesive | 14 February, 2003

I sent you some adhesive printing application data from MPM and Epibond for review. There's good stuff in docs. Run the ppt file as a Show to get the animation.

reply »

blnorman

#23400

Screen printing adhesive | 14 February, 2003

We currently use Epibond 7275 with MPM printers. Unfortunately we've had problems with Vantico (formerly Ciba) providing a consistent product. Last summer we had extreme difficulty printing due to excessively high adhesive viscosity (20% higher than our spec maximum allowable).

reply »

#23405

Screen printing adhesive | 14 February, 2003

We use Thermoset MA-420 on a pair of Elite 6920 printers. Excellent results. It took some experimentation with aperture sizes and stencil thickness but it works great.

reply »

btoleno

#23423

Screen printing adhesive | 19 February, 2003

I have a paper that was presented at the SMTA technical session at Nepcon West in Dec on screen printing adhesives. If you would like a copy send me an e-mail at brian.toleno@loctite.com and I can send you an electronic copy.

reply »

Brian Doyle

#23438

Screen printing adhesive | 20 February, 2003

If you have it in electronic copy you should post it to the SMTnet library.

reply »

pcb components vacuum pick up

On-board Dispensing of Dots & Lines