LED's TOMBSTONING

Terry Saunders

#25130

LED's TOMBSTONING | 10 July, 2003

ALL,

WE ARE HAVING TOMBSTONING ISSUES WITH LED'S -ANY HELP OUT THERE.

PLEASE ADVISE.

TERRY SAUNDERS.

This message was posted via the Electronics Forum @

reply »


RDR

#25135

LED's TOMBSTONING | 10 July, 2003

Search the archives. There is a ton of tombstone discussion in there.

Russ

reply »

#25140

LED's TOMBSTONING | 11 July, 2003

Hi there is one thing. I had the same problem before and after examine it I found the problem is in the pads. The pads on the board were bigger then usual and the distance between them also was a little bit longer.Theese two are the best preconditions for tombstoning. If it's not that all others things were said in the forum not long ago.