WHERE TO BUY ALUMINUM TAPE FOR PROFILING?

James

#25210

WHERE TO BUY ALUMINUM TAPE FOR PROFILING? | 17 July, 2003

COULD ANYONE TELL ME WHERE TO BUY ALUMINUM TAPE USED FOR PROFILING? THANKS FOR YOU INPUT.

reply »

#25211

WHERE TO BUY ALUMINUM TAPE FOR PROFILING? | 17 July, 2003

Aluminum tape suppliers: * Chomerics Inc (T405 aluminum tape) 77 Dragon Ct # A Woburn, MA 01801 (781) 935-4850 * CS Hyde Company 800-461-4161 / 847-265-6903 Fax: 800-441-8063

reply »

#25252

WHERE TO BUY ALUMINUM TAPE FOR PROFILING? | 22 July, 2003

You can also get it through Contact East.

reply »

Dean

#25292

WHERE TO BUY ALUMINUM TAPE FOR PROFILING? | 29 July, 2003

KIC Thermal Profiling also sells the double - sided aluminum tape. They also did a white paper characterizing the material...

Good stuff.