#25955

About immersion tin | 5 October, 2003

Hi all: I want to know the parameter and criterion about the process of immersion tin,could you be kindly to give me the hins about it in more detail.Thank you for your support. Best wishes christ

reply »

#25961

About immersion tin | 6 October, 2003

While you are waiting for others to reply, search the fine SMTnet Archives on: * immersion and tin * imm and tin

reply »

christ

#25996

About immersion tin | 8 October, 2003

Hi Dave: Thanking in advance for your valuable response!