Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


High-temperature thermal profiling adhesive

Ron W

#26812

High-temperature thermal profiling adhesive | 9 January, 2004

I'd like to know if anyone could recommend a good high-temperature adhesive that can be used for thermocouple attachment. I've always used high-temp solder and tape in the past, but would like to try using adhesive. Any info is certainly appreciated.

reply »

Dean

#26815

High-temperature thermal profiling adhesive | 9 January, 2004

How high are we talking? 1000 Celsius?

KIC Thermal Profiling double sided aluminum profiling tape. I have used at an extreme application of 240 to 300 degrees celsius for 18 minutes. With up to 30 passes with no visible degree of deterioration. Good stuff

reply »

#26817

High-temperature thermal profiling adhesive | 10 January, 2004

We have always had success with light cure adhesives for probe attachment.

Try these guys for some samples. http://www.dymax.com

reply »

#26824

High-temperature thermal profiling adhesive | 12 January, 2004

We use a product here made by Loctite. Its Loctite 383 thermal adhesive. It works fine.

Steve

reply »

Precision Auger Dispense Pump