Tinning Gold Parts | 24 May, 2004

I am interested in how Military / Class 3 manufacturers are handling Gold SMT components. We are receiving an increasing number of tape and reel components that are gold plated. Per J-STD we need to tin all gold components. Are parts being removed from tape and reel or tube, tinned, cleaned and then mounted? Some of these components do not lend themselves to tinning at all - small size etc. Ideally these parts would come in already tinned. How are others handling this?

reply »

#28757

Tinning Gold Parts | 24 May, 2004

I know some are using Tintronics in Alabama. http://www.tintronics.com/

reply »

#28764

Tinning Gold Parts | 25 May, 2004

Additional tinning service providers are: * Source Electronics 26 Clinton Drive, Hollis, NH 03049; 603-595-2906 Fax: 603-595-0068 800-227-2909 http://www.sourcee.com

* Six Sigma; 905 Montague Expressway, Milplitas, CA 95035; 408-956-010; FAX 408-956-0199; http://www.sixsigmaservices.com

* Meehan Electronics; 191 River Rd.,Clarksburg, MA 01247; 413-664-9377 Fax 413-663-6048 http://www.meehanelectronics.com

* XL Addenda;; 708.971.8843fax8846; Gene Binkowski * Corfin Industries; 7B Raymond Ave, Unit 7 Salem, NH 03079; 603-893-9900 fax 6800 http://www.corfin.net admin@corfin.net Thomas Hamel * Chip Pro; 10390 E. Lakeview Dr #206 Scottsdale, AZ 85258; 480-860-5790 Fax 8366 [Processing Facility; 1610 No. Freeway 35E #214 Carrollton, TX 75006; 972-242-9455 fax 8497] http://www.chipro.com