reworking BGAs

Jacqueline Coia

#3889

reworking BGAs | 6 June, 2000

Hi There, Could someone please point me in the right direction in the subject of baking 'metal' packaged BGAs before rework. What are recommended baking temp. & time.

Much appreciated. Jack

reply »

khalid

#3890

Re: reworking BGAs | 6 June, 2000

Please refer to the following document for your information. IPC/JEDEC J-STD-003. This document can be downloaded from WWW.IPC.ORG. Feel free to contact me if you have any question. Khalid.Saeed@marconi.com