epoxy for other than water tight seals

#29860

epoxy for other than water tight seals | 5 August, 2004

Is there a specific epoxy that is most suitable for sealing a polycarbonate chamber, which will have hydrogen flowing through it at no greater than 10psi? Can any epoxy that provides a watertight seal be used for hydrogen applications?

We have the following epoxies available at the moment: [1] Devcon 2 Ton Clea Epoxy [2] Circuit Works Conductive Epoxy [3] Super Glue corporations Quick Setting Epoxy Are any of these good for our purpose?