where be located while embed the thermocouple into PTH hole ? | 9 September, 2004

A fresher goes in SMTonline ,I would like to learn the knowledge that how to embed and high temp. solder thermocouple into PTH hole while profiling board ,where the bead of T.C be located ,whether in PTH hole or protrude the bottom surface of board .thanks in advance .

reply »

#30500

where be located while embed the thermocouple into PTH hole ? | 14 September, 2004

Try: 7530 - Guidelines for Temperature Profiling for Mass Soldering (Reflow and Wave)