Selective soldering

John

#30662

Selective soldering | 23 September, 2004

Have anyone experience with temp.profile for selective soldering?Could you give me more information about that?

Thank you!

reply »

C Lampron

#30692

Selective soldering | 24 September, 2004

Hi John,

We have been selective soldering for about two years. My suggestion is to use the same guidelines for preheat, duration and temp as you would in wave. Your flux manufacturer should be able to provide you with the details.

Good Luck

Chris

reply »