Temp. Specs on SMT parts

#31512

Temp. Specs on SMT parts | 29 November, 2004

I would like to know if anyone has a generic Temp. chart for SMT components. I need to know the Max. temp. parts can withstand while going through the reflow or wave operations.

Thanks Bob Leible Raven Industries

reply »


RDR

#31517

Temp. Specs on SMT parts | 29 November, 2004

IPC 782 has some info in it by package type. This is usually dictated by each component manufacturer. All SMT parts should be able to withstand 220 C for at least 60 sec.

Russ