solder pad with nickel plating | 11 May, 2005

i want to know which type of solder paste and reflow profile can support the solder pad with nickel but not covered gold on the pcb.

reply »


RDR

#34196

solder pad with nickel plating | 11 May, 2005

I would contact your paste supplier, bare nickel can be impossible to wet to. How oxidized is it?

reply »


Rob

#34209

solder pad with nickel plating | 12 May, 2005