Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Bga question??

techknow..

#34903

Bga question?? | 12 June, 2005

When examining a Bga using an Ersascope, I found that all the joints where good. However I found that the first few solder balls from left to right ( vice versa ) seem higher than the middle solder balls. It appears that the body of the part is flexing upwards on these solder balls. Can anyone explain this to me ?

Thanks in advance.

reply »

Bob R.

#34910

Bga question?? | 13 June, 2005

BGAs warp during reflow. When balls solidify they lock the device into this warped state. It's not a big deal until the warp gets severe enough that you have opens and/or shorts.

reply »

peter ng

#34922

Bga question?? | 13 June, 2005

The placing stroke(mounting press) of the BGA may be too high.Try to reduce the value at the component data.

reply »