Solder Tank For Lead Free wave soldering m/c

Charls R

#35361

Solder Tank For Lead Free wave soldering m/c | 7 July, 2005

Hello friends, We have wave soldering m/c Stainless Steel Solder tank. We have in process to chengeover to Lead Free Tank. As for as my concern Titanium coating to tank is one solution. Is there any otehr metal alloy tank is available? if yes what should be the metal alloy . Please help me .

reply »

Charls R

#35362

Solder Tank For Lead Free wave soldering m/c | 7 July, 2005

Hello friends, We have wave soldering m/c Stainless Steel Solder tank. We have in process to chengeover to Lead Free Tank. As for as my concern Titanium coating to tank is one solution. Is there any otehr metal alloy tank is available? if yes what should be the metal alloy . Please help me .

reply »


G S

#35365

Solder Tank For Lead Free wave soldering m/c | 7 July, 2005

Yes there are other solutions. Call me at 903-892-5636 to discuss. Glenn

reply »

#35386

Solder Tank For Lead Free wave soldering m/c | 8 July, 2005

Hello we manufacture titanium retrofit kits with a 5mm titnaium tank we have done 7 conversions for Sony , Wahl in Hungary , Fextronics in Ireland without any problems at all. If you require additional information please do not hesitate to contact me on +44 (0) 1792 885594

Robert Emanuel Teilo Engineering Ltd

reply »

#35394

Solder Tank For Lead Free wave soldering m/c | 8 July, 2005