wave solder upgrade | 11 October, 2005

Hi,

I'm wondering what the average price of a conversion on a wave solder oven from leaded to lead free is in the uk, has anyone had theirs done recently? Would you let me know roughly what it cost? any help would be appreciated.

regards

Dougs

reply »

#37203

wave solder upgrade | 18 October, 2005

Hi Doug

We manufacture conversion kits completley out titanium. We would be happy to give you a quote. Please visit http://wwwteiloengineering.com where you will find our contact details.

Best Regards

Mike Emanuel

reply »

KEN

#37217

wave solder upgrade | 19 October, 2005

I had one machine converted 3 years ago. The cost was $30K (US) but that included a total refurbishment because the machine was not cleaned and maintained well.

reply »