Please give us some ideas on some critical parameters in checking the solder paste shape, size & volume after Solder Paste Printing.

reply »

#38325

Inspection Criteria | 8 December, 2005

Satisfactory solder paste should: * Be aligned with all pads * Conform to the stencil pad-aperture size * Have a smooth, flat void-free surface